Turret Slitter Rewinder

Turret Slitter Rewinder

Slitting machine shutdown operation
1. After the cutting is completed, the unloading is stopped;
2. Release the switch and lift the cutter unit.
3. Clean the crimping device and turn off the curling blower.
4. Turn off the photoelectric tracking system.
5. Turn off the power and air supply of the whole machine.
6. Clean up the surrounding environment.
7. Carefully fill in the production daily record, product self-checklist and other work records.

Turret Slitter Rewinder

Reasons, countermeasures and effects of BOPP film slitting quality ---

Fives. Multilateral
Although the polygon and the end face are not the same as the faulty end faces of some layers of the film roll, the two are different. The unevenness of the end face is the jagged phenomenon that occurs when the film width is not changed, and the multilateral product The film width is slightly wider than the normal size.

1. Multilateral impact on quality of use
The impact of multilateral use on the end is basically the same as that of the end face, mainly to track the problem of alignment and the impact on the appearance of the product.

 

 

Turret Slitter Rewinder

Reasons, countermeasures and effects of BOPP film slitting quality ---

ten. Color circle
The color circle is caused by a certain degree of contamination inside or outside the film, which causes the quality of the color circle on the end face of the film roll after slitting and winding. Membrane surface pollution sources come from two aspects. One is the film-forming process. The color circles generated in the front part of the film, such as raw materials, feeding systems, extrusion systems, and die flow channels, generally cause pollution to the inside of the film (core layer). Some color-circle products can clearly observe a large amount of fish-eye impurities in the film. The color circles generated in the film-forming stage and the slitting process mainly cause pollution to the outside (surface) of the film, but whether it is internal or external pollution, It is impossible to remove the impurities from the contaminated film and restore the original appearance. The product with serious color circle has low transparency, the film color is different from the normal product, and it can not be used at all. It can only be reduced to other external treatments, while the products with slight color circles are It has little effect on the transparency of the product and does not affect the use effect of the single film. However, due to the inconspicuous appearance of the color circle product, the “selling phase” is poor, which has a great influence on the image of the German brand. It is not suitable for direct delivery. Secondary processing. If the color circle is caused by external dust pollution factors, the dust will be adsorbed on the surface of the film, resulting in poor quality of heat sealing and poor laser compression.