Sellotape Cutting Machine

Reasons, countermeasures and effects of BOPP film slitting quality ---

 

six. Burr
Most of the reason for the burrs is that the cutting knife is too blunt, and replacing the cutter can solve the problem. Different types of films have different degrees of wear and tear on the cutters. The thicker the thickness, the greater the wear on the cutters, and the wear of the cutters due to the titanium dioxide and other materials. It is fast, so it is necessary to adjust the blade cutting position or replace the blade according to different cutting objects in time to avoid the appearance of raw products. Due to the high cost of cutting the raw edge product (retrocuting processing cost and edge material loss), it is much higher than the value of the scrapping blade. Therefore, preventive measures should be taken, and the replacement cycle of the blade should be budgeted. Adjust or replace the blade before the problem occurs. Blades reduce losses.
 

Sellotape Cutting Machine

Reasons, countermeasures and effects of BOPP film slitting quality ---

Eight. Indentation
There are two reasons for the cause of film roll indentation. One is caused by the winding wheel of the film forming process, and the other is caused by the cutting factor. The reasons for the cutting are:
1 Due to the poor adjustment of the angle of the puller wheel, the pressure and tension of the puller wheel are concentrated on one point of the film, and the friction of the contact point causes damage to the film surface to form an indentation.
2 The winding roller is damaged, such as scratches, etc., the degree of film roll indentation is large when the scratch is longitudinal; 3 The winding roller is contaminated, causing the surface of the pressure roller to be uneven, such as adhesive tape, impurities, etc. It will also cause the film roll to be indented and the press roll must be cleaned.
Slight indentation does not affect the use of the product, but it affects the appearance of the product, causing the customer to doubt the quality of the product; the obvious indentation not only affects the appearance of the product, but also attenuates the corona value of the film, affecting the film. Processing performance.