Tape slitter setting control:
1. Set the slitting menu according to the type, thickness, length, width, etc. of the film arranged in the slitting plan.
2. Lift the corresponding BOPP film file from the PDF.
3. Set the winding length and width of the film of the corresponding specification.
4. Select the corresponding winding station, adjust the pressure roller arm and pressure roller, and install the paper core of the corresponding specifications.

1300mm Packaging Tape Slitter

Reasons, countermeasures and effects of BOPP film slitting quality ---

three. Irregular end faces
The end face irregularity refers to the unevenness of the end face which occurs when the film width is constant. The end face is generally in two forms: one is that the end faces are irregularly jagged, and the other is a regular wave-shaped irregularity.
1. Causes and countermeasures for uneven end faces:
1 The cutting parameters are not well adjusted. For example, if the cutting speed and the sheet/pressure are poorly matched, the sheet/pressure curve should be set according to the slitting speed;
2 abnormal vibration of the cutting device, overhaul;
3 divided and unwinding rolls are unbalanced and adjusted;
4 The parameters of the winding arms at both ends are inconsistent, and the force distribution of the winding process affects the flatness of the end face, usually the wavy end faces are not aligned and overhauled;
5 The influence of film properties, such as smoothness, etc., Ts, Pm and other models are more prominent, and the cutting parameters should be set according to different film characteristics;
6 film thickness is uneven;
7 Wrinkling during the slitting process will also cause unevenness of the end face and adjust the flattening film;
8 If the film is too static, improve the electrostatic properties of the film or check if the static eliminator of the slitter is invalid.

1300mm Packaging Tape Slitter

Reasons, countermeasures and effects of BOPP film slitting quality ---

ten. Color circle

The factors that cause the film to roll the color circle are:
(1) Contamination equipment is contaminated: due to the pollution of the dust in the cutting workshop, as well as the operation of the equipment in the slitting process and the friction between the membrane and the friction generated by the static electricity, the cutting equipment continuously accumulates more and more dust. When it accumulates to a certain extent and fails to clean in time, it will pollute the slit film roll to form a color circle. In addition, the aging and hardening of the roll skin (sand) debris will also cause the color circle of the film roll to appear.
(2) The environment of the cutting environment is polluted: during the cutting process, due to the influence of some accidental pollution sources, such as the dust on the ceiling of the cutting machine, the exhaust of the diesel forklift, etc., the air is spread to pollute the cutting products. And form a color circle.
In order to effectively reduce the impact of color circles on product quality, the following measures must be taken:
(1) Do 5S work regularly to maintain the sanitation of the workshop and the cleanliness of the machine; (2) It is forbidden to open the doors and windows without sand filter for a long time, and keep the good habit of closing the door;
(3) The contaminated film on the surface of the parent roll must be removed before the film can be cut, so as to avoid the dirt of the surface film from contaminating the cutting machine;
(4) The diesel forklift that requires black smoke is kept away from the surrounding of the workshop to prevent the tail gas pollution from being cut into the products.