Automatic Line Bopp Tape Slitter Rewinder Machine

Automatic Line Bopp Tape Slitter Rewinder Machine

Inspection and preparation before the cutting machine is turned on
4.1.1. Confirm that the main power supply voltage is 380V.
4.1.2. Turn on each power switch and check if the electricity and gas supply are normal.
4.1.3. Before starting the machine, you must confirm that the surface of each guide roller is smooth and free of burr dust, debris, etc. When cleaning the machine, use alcohol or water to soft cloth.
Wipe, can not be wiped with other solvents, remove the impurities around the equipment and production, to ensure normal production;
4.1.4. Obtain all kinds of accessories and tools such as slitting products and tapes in strict accordance with the production instruction sheet and the process card requirements.
4.1.4.1. Receive the composite film specified on the production instruction sheet, check whether the composite film tracking card is complete, and describe the previous quality problem is it clear.
4.1.4.2. Confirm the cut specifications, roll direction, batch number, material structure, winding diameter or meter number according to the production order. 4.1.5. Carefully check the equipment to confirm that each rewinding mechanism, EPC device, and tension control system are normal, and confirm static electricity.
Whether the elimination is normal or not;
4.1.6. The unwinding material is ready, and then the film is routed in the correct way;
4.1.7. Prepare the winding paper core according to the slitting specifications and place it in the corresponding position of the winding reel.

Automatic Line Bopp Tape Slitter Rewinder Machine

Reasons, countermeasures and effects of BOPP film slitting quality ---

nine. Scratch
      Whether the slitting and scratching can be compared and determined by the film surface before and after the slitting, there are various reasons for the scratching of the membrane surface, and the analysis should be based on the appearance of the scratch, such as short-line scratching. The difference of the speed ratio of each drive roller exceeds the process setting requirement, and it needs to be carefully tested and adjusted. If the film surface scratch occurs continuously, the film on the slitter should be inspected for whether it touches the fixed object or cuts each. Whether the roller adheres to dirt such as fine sand grains scratches the film surface.
Scratch is the appearance quality problem of the film, which directly affects the quality appearance of the deep-processed product. Therefore, it is not allowed to exist in the film quality control standard. The slitting process finds that the scratching problem must be carefully checked and quickly eliminated. Since the scratch on the film surface is an irreversible appearance quality problem, it is not allowed to operate the disease when the film surface is scratched, so as to avoid the continuous occurrence of the problem.
      

Automatic Line Bopp Tape Slitter Rewinder Machine

Reasons, countermeasures and effects of BOPP film slitting quality ---

ten. Color circle

The factors that cause the film to roll the color circle are:
(1) Contamination equipment is contaminated: due to the pollution of the dust in the cutting workshop, as well as the operation of the equipment in the slitting process and the friction between the membrane and the friction generated by the static electricity, the cutting equipment continuously accumulates more and more dust. When it accumulates to a certain extent and fails to clean in time, it will pollute the slit film roll to form a color circle. In addition, the aging and hardening of the roll skin (sand) debris will also cause the color circle of the film roll to appear.
(2) The environment of the cutting environment is polluted: during the cutting process, due to the influence of some accidental pollution sources, such as the dust on the ceiling of the cutting machine, the exhaust of the diesel forklift, etc., the air is spread to pollute the cutting products. And form a color circle.
In order to effectively reduce the impact of color circles on product quality, the following measures must be taken:
(1) Do 5S work regularly to maintain the sanitation of the workshop and the cleanliness of the machine; (2) It is forbidden to open the doors and windows without sand filter for a long time, and keep the good habit of closing the door;
(3) The contaminated film on the surface of the parent roll must be removed before the film can be cut, so as to avoid the dirt of the surface film from contaminating the cutting machine;
(4) The diesel forklift that requires black smoke is kept away from the surrounding of the workshop to prevent the tail gas pollution from being cut into the products.

About

Zhengzhou EAST IMPORT AND EXPORT co., ltd . ( a goulian group of company) a manufacturer and exporter for all kind of packaging machinery , like bopp tape coating machines, bopp tape slitting machines. Bopp tape core cutter, bopp tape core loader etc

Got any Questions?
CALL US NOW

+86-17744612788

gl006@guolianjixie.com