Slitting Adhesive Tape Machinery

Slitting Adhesive Tape Machinery

Slitting adjustment
1. Put the cutter down, open the curling blower switch, set the winding tension, start the machine, run 2-3 meters, stop;
2. Measure the width of each joint to confirm whether the requirements are met. If there is any error, the ratio of the cutter should be re-matched.
3. Check whether each of the paper cores and the corresponding film are aligned, otherwise adjust them;

Slitting Adhesive Tape Machinery

Causes, countermeasures and effects on the quality of BOPP film slitting quality ---

(iv) Effect of film roll tightness on product quality
1. The winding is too tight:
1 fluttering/starting bone: As BOPP film, it is normal for the thickness of the product to fluctuate within a reasonable range. If the reeling tightness is appropriate, this thickness fluctuation will not affect the quality of use, but when the slitting is too tight The thicker layers of the film are stacked together to cause edge thickness or bone swelling, which affects the quality of use. The fluttering or bone formation that is formed by over-tightening is often difficult to find during the slitting process, but after the product has been stored for a period of time, the problem will be highlighted. In addition, there are several types of products with uneven thickness defects that can be easily revealed, such as ultra-transparent tape film, crystal film, heat sealing film, etc., while fluttering and bone-starting phenomenon will cause different quality of all film products. The degree of influence, especially for products that require printing and processing, is particularly prominent.
2 Adhesion: over-tightening of double-sided corona products, anti-corona products and products with less anti-adhesive content will cause adhesion quality problems, and the problem can only be found in the customer's use, the impact is great, and appears Products with adhesion problems can only be disposed of as scrapping, causing large losses to the company.
3 Face wrinkles: Due to the tight winding, the film cushioning performance is degraded. The wrinkles formed by the extrusion of the film on the end face of the product during handling and loading and unloading are difficult to eliminate, forming the end wrinkles and affecting the quality of the product.
4 Pitting: Due to the tightness of the winding, the film near the paper tube is affected by the rough surface of the paper tube, which causes pitting, which affects the quality of the product. The use of the polished paper tube will eliminate the surface of the film and improve it. Start wrinkles).

Slitting Adhesive Tape Machinery

Reasons, countermeasures and effects of BOPP film slitting quality ---
two. Wrinkles (wrinkles, vertical wrinkles, cross wrinkles, wrinkles)

 

(2) Causes and countermeasures of longitudinal wrinkles
Longitudinal wrinkles mean that the surface of the film roll forms a circumferential rib line. In the process of slitting, a large amount of air entrapment or cumulative thickness unevenness is the main cause of longitudinal streaks, and it is difficult to eliminate the occurrence of a relatively serious stripe. When the longitudinal wrinkles appear in the slitting process, the tension is reduced and the pressure is applied to discharge the air in the film roll to improve the longitudinal wrinkle problem. However, the adjustment range should consider the impact on wrinkles and other aspects (according to relevant professional information, longitudinal wrinkles One of the reasons is that the slitting speed is too fast, and the film roll is most prone to the quality problem of the longitudinal stripe at high speed, but there is no obvious influence in actual production, which remains to be studied). Another reason for the vertical wrinkles is the influence of the running accuracy of the equipment. For equipment with high requirements for running accuracy, after a long period of continuous use, the running accuracy of some components has decreased. For large slitting machines, it is more difficult to ensure the running accuracy due to the large number of running parts. Moreover, since the plastic film is a polymer product, its thickness is very thin, and it is more susceptible to damage during processing. Therefore, once the running accuracy is insufficient, quality problems such as vertical streaks are likely to occur. For this reason, it should be cautious when replacing equipment parts and accessories. It is advisable to use durable and high-precision parts, and it must also ensure a certain precision during installation. Otherwise, it is difficult to meet the operation requirements of the slitting machine.
The flattening roller flattens the film and eliminates some of the longitudinal wrinkles produced by the film under tensile stress.
(3) Causes and countermeasures of cross wrinkles
In addition to the influence of the parent-rolling factor, the transverse wrinkles of the film are mainly caused by the sag-like transverse wrinkles produced by the loosening of the slit film roll. Generally, the slitting process is effective in reducing the wrinkles and reducing the pressure, and should be effective for different types of products. Adjusting the slitting and pressure can effectively eliminate the occurrence of cross wrinkles.