Slitting adjustment
1. Put the cutter down, open the curling blower switch, set the winding tension, start the machine, run 2-3 meters, stop;
2. Measure the width of each joint to confirm whether the requirements are met. If there is any error, the ratio of the cutter should be re-matched.
3. Check whether each of the paper cores and the corresponding film are aligned, otherwise adjust them;

Bopp Rewinder And Slitter

Reasons, countermeasures and effects of BOPP film slitting quality ---

three. Irregular end faces
The end face irregularity refers to the unevenness of the end face which occurs when the film width is constant. The end face is generally in two forms: one is that the end faces are irregularly jagged, and the other is a regular wave-shaped irregularity.
1. Causes and countermeasures for uneven end faces:
1 The cutting parameters are not well adjusted. For example, if the cutting speed and the sheet/pressure are poorly matched, the sheet/pressure curve should be set according to the slitting speed;
2 abnormal vibration of the cutting device, overhaul;
3 divided and unwinding rolls are unbalanced and adjusted;
4 The parameters of the winding arms at both ends are inconsistent, and the force distribution of the winding process affects the flatness of the end face, usually the wavy end faces are not aligned and overhauled;
5 The influence of film properties, such as smoothness, etc., Ts, Pm and other models are more prominent, and the cutting parameters should be set according to different film characteristics;
6 film thickness is uneven;
7 Wrinkling during the slitting process will also cause unevenness of the end face and adjust the flattening film;
8 If the film is too static, improve the electrostatic properties of the film or check if the static eliminator of the slitter is invalid.

Bopp Rewinder And Slitter

Reasons, countermeasures and effects of BOPP film slitting quality ---

 

six. Burr

Another reason for the burrs is the quality of the parent roll.
First, when the mother roll product is wrinkled, the burr phenomenon is likely to occur when the film is cut to the sipe roll and the film is not effectively flattened;
Second, when the film is thick or thin for a long time, the film is prone to burr phenomenon when the film is not attached to the sipe, especially in the triangular position of the thickness. In addition, since the thinner the film, the lower the stiffness, and the higher the chance of burrs.

About

Zhengzhou EAST IMPORT AND EXPORT co., ltd . ( a goulian group of company) a manufacturer and exporter for all kind of packaging machinery , like bopp tape coating machines, bopp tape slitting machines. Bopp tape core cutter, bopp tape core loader etc

Got any Questions?
CALL US NOW

+86-17744612788

gl006@guolianjixie.com