Bopp Automatic Slitting Machine

Bopp Automatic Slitting Machine

Slitting adjustment
1. Put the cutter down, open the curling blower switch, set the winding tension, start the machine, run 2-3 meters, stop;
2. Measure the width of each joint to confirm whether the requirements are met. If there is any error, the ratio of the cutter should be re-matched.
3. Check whether each of the paper cores and the corresponding film are aligned, otherwise adjust them;

Bopp Automatic Slitting Machine

Reasons, countermeasures and effects of BOPP film slitting quality ---

Seven. Sharp edge
The curling occurs at the edge of the film winding, which causes the curling. The reason is that the edge of the thick film is curled up and the edge part is lifted up; the second is that the winding is too tight, and the tension can be shortened by slitting. Speed ??to improve the resulting edge curling phenomenon; third, the cutter is too blunt, and the stretching phenomenon occurs at the slit when slitting, causing the edge of the film roll to be turned outwards after winding to cause the curling edge, and the cutting should be replaced in time. The knife can avoid the occurrence of the curling problem; the fourth is that the tool is not installed correctly, such as the blade is close to the edge of the sipe and the blade is passivated. Cutting with a round knife can improve the curling of the film roll.
In the use of the unwinding process, there will be different degrees of side-floating in the unwinding process, and it is impossible to track the alignment with the electric eye, which directly affects the use effect. Therefore, it is necessary to change the product with the curled edge.

Bopp Automatic Slitting Machine

Reasons, countermeasures and effects of BOPP film slitting quality ---

ten. Color circle

The factors that cause the film to roll the color circle are:
(1) Contamination equipment is contaminated: due to the pollution of the dust in the cutting workshop, as well as the operation of the equipment in the slitting process and the friction between the membrane and the friction generated by the static electricity, the cutting equipment continuously accumulates more and more dust. When it accumulates to a certain extent and fails to clean in time, it will pollute the slit film roll to form a color circle. In addition, the aging and hardening of the roll skin (sand) debris will also cause the color circle of the film roll to appear.
(2) The environment of the cutting environment is polluted: during the cutting process, due to the influence of some accidental pollution sources, such as the dust on the ceiling of the cutting machine, the exhaust of the diesel forklift, etc., the air is spread to pollute the cutting products. And form a color circle.
In order to effectively reduce the impact of color circles on product quality, the following measures must be taken:
(1) Do 5S work regularly to maintain the sanitation of the workshop and the cleanliness of the machine; (2) It is forbidden to open the doors and windows without sand filter for a long time, and keep the good habit of closing the door;
(3) The contaminated film on the surface of the parent roll must be removed before the film can be cut, so as to avoid the dirt of the surface film from contaminating the cutting machine;
(4) The diesel forklift that requires black smoke is kept away from the surrounding of the workshop to prevent the tail gas pollution from being cut into the products.